{"id":28258,"date":"2020-05-28T13:45:00","date_gmt":"2020-05-28T11:45:00","guid":{"rendered":"https:\/\/delta-engineering.be?p=28258"},"modified":"2025-05-26T11:12:35","modified_gmt":"2025-05-26T09:12:35","slug":"l-ring-drums-plasma-coater","status":"publish","type":"post","link":"https:\/\/marketing.delta-engineering.be\/delta\/l-ring-drums-plasma-coater","title":{"rendered":"DPC133"},"content":{"rendered":"<h2 class=\"m_title\">Plasma coater for L-ring drums<\/h2>\n\n&nbsp;<\/p>\n<h4><strong>What is plasma coating?<\/strong><\/h4>\n<p>PECVD is short for &#8216;plasma enhanced chemical vapour deposition&#8217;. It uses electrical discharge (in a low vacuum pressure condition) to <strong>decompose a gas<\/strong>. By doing so, it <strong>creates a thin coating layer on the inside wall of the L-ring drum<\/strong>.<\/p>\n<p>Besides, plasma coating is an environmentally friendly way to create fully recyclable coated products. They can have different physical and\/or chemical properties. These depend on the material and the plasma gas used.<\/p>\n<p>You can obtain different properties:<\/p>\n<ul>\n<li><strong>modify<\/strong> the <strong>surface tension<\/strong> for <strong>better sliding, adhesion, wettability<\/strong><\/li>\n<li><strong>improve<\/strong> the <strong>barrier<\/strong> in different applications: <strong>migration, permeation&#8230;<\/strong><\/li>\n<\/ul>\n<p>&nbsp;<\/p>\n<h4><strong>Plasma coating, the environmentally friendly approach!<\/strong><\/h4>\n<p>As you may know, new legislation is on its way. It will require ambitious <strong>recycling of packaging material<\/strong>.<br \/>\nThat is challenging for multilayers, because they provide good barrier properties, but are non-recyclable because of their different, inseparable layers.<br \/>\nOur plasma coater can create <strong>better barrier properties than multilayers<\/strong>. But you may consider it as a <strong>monolayer packaging<\/strong>.<\/p>\n<p>It is <strong>easy to grind the coated material and recycle<\/strong> it, together with non-coated materials:<\/p>\n<ul>\n<li>The <strong>percentage<\/strong> of our <strong>coating<\/strong> is <strong>negligible<\/strong> to that of the plastic packaging: 60 to 150 nanometers.<\/li>\n<li>The coating will be <strong>largely removed during the washing process<\/strong>.<\/li>\n<li>Coated L-ring drums will not reach a market penetration much higher than 10 %. As a result, this <strong>rules out a change in flake quality<\/strong> in the recycling plants.<\/li>\n<\/ul>\n<p>We <strong>only use environmentally friendly gases<\/strong> for plasma coating.<br \/>\n&nbsp;<br \/>\nFurthermore, the gases are largely consumed during the process, <strong>reducing the exhaust<\/strong> to a minimum. In addition, an <strong>active carbon filter<\/strong> can easily capture the remainder of the gases, should local legislation require this.<br \/>\n&nbsp;<\/p>\n<h4><strong>The machine<\/strong><\/h4>\n<p>The DPC133 is a plasma coater for L-ring drums. It is designed to be integrated into an L-ring blow moulding line. The machine robot has to insert\/extract the products. Before inserting the L-ring drums into the vacuum chamber, the machine vacuumises both.<br \/>\nThis plasma coater can coat <strong>L-ring drums from ca. 50L up to 250L<\/strong>.<\/p>\n<p>The machine can use 2 technologies:<\/p>\n<ul>\n<li>Carbon deposition on PET containers. This results in an improved O2 ( &gt;30x) barrier, CO2 ( &gt;7x) and H20 ( &gt;2x).<\/li>\n<li>Carbon Fluor deposition. This results in a \u00e2\u20ac\u02dcfluorinated\u00e2\u20ac\u2122 container without actually using any Fluor.<\/li>\n<\/ul>\n<p>This is a <strong>single vacuum chamber<\/strong> machine. It can treat around <strong>35-55 L-ring drums per hour (HDPE)<\/strong> or <strong>50-110 drums per hour (PET)<\/strong>, depending on the process and volume.<br \/>\nHowever, these speeds are indicative, so please use our <a href=\"\/?p=24466\" target=\"_blank\" rel=\"noopener noreferrer\">calculation tool<\/a> to simulate the exact speed, power and gas consumption.<\/p>\n<p>The plasma coater for L-ring drums uses proprietary technology. Therefore, we only disclose limited info on our website. So please contact us for more information.<\/p>\n<p>We can develop specific barrier processes depending on your needs.<\/p>\n<p>&nbsp;<\/p>\n<h4><strong>ADVANTAGES<\/strong><\/h4>\n<ul>\n<li>Weight reduction of the L-ring drums<\/li>\n<li>We can adjust the barrier to your needs<\/li>\n<li>100 % recyclable<\/li>\n<li>Can treat PET &amp; HDPE containers<\/li>\n<li>On PET: Improved Oxygen barrier<\/li>\n<li>On HDPE: Improved Solvent barrier<\/li>\n<\/ul>\n<p>Please download our <a href=\"\/\/marketing.delta-engineering.be\/delta\/wp-content\/uploads\/2020\/06\/Plasma-coating-brochure_UK_2019_V1.pdf\" rel=\"noopener noreferrer\" target=\"_blank\">Technology brochure<\/a> for a full overview.<br \/>\n&nbsp;<\/p>\n<h4><strong>OTHER VERSIONS<\/strong><\/h4>\n<p>Container plasma coater: <a title=\"DPC123\" href=\"\/?p=23230\" target=\"_blank\" rel=\"noopener noreferrer\">DPC123<\/a>, <a title=\"DPC223\" href=\"\/?p=23245\" target=\"_blank\" rel=\"noopener noreferrer\">DPC223<\/a>, <a title=\"DPC413\" href=\"\/?p=23268\" target=\"_blank\" rel=\"noopener noreferrer\">DPC413<\/a>, <a title=\"DPC613\" href=\"\/?p=23340\" target=\"_blank\" rel=\"noopener noreferrer\">DPC613<\/a><br \/>\nBottle plasma coater: <a title=\"DPC403\" href=\"\/?p=25354\" target=\"_blank\" rel=\"noopener noreferrer\">DPC403<\/a><br \/>\n\n\n\n\n\n\n\nPRICE\n\n\n\nRESOURCES\n\n\n\n","protected":false},"excerpt":{"rendered":"<p><b>Plasma coater for L-ring drums<\/b><\/p>\n<p>This plasma coater can coat plastic L-ring drums from ca. 50L up to 250L. It creates a barrier on the inside of PET (50-110 BPH) and HDPE (35-55 BPH) drums. Fully recyclable coating. Single vacuum chamber machine.<\/p>\n","protected":false},"author":4146,"featured_media":42346,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":[],"categories":[1880],"tags":[],"_links":{"self":[{"href":"https:\/\/marketing.delta-engineering.be\/delta\/wp-json\/wp\/v2\/posts\/28258"}],"collection":[{"href":"https:\/\/marketing.delta-engineering.be\/delta\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/marketing.delta-engineering.be\/delta\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/marketing.delta-engineering.be\/delta\/wp-json\/wp\/v2\/users\/4146"}],"replies":[{"embeddable":true,"href":"https:\/\/marketing.delta-engineering.be\/delta\/wp-json\/wp\/v2\/comments?post=28258"}],"version-history":[{"count":18,"href":"https:\/\/marketing.delta-engineering.be\/delta\/wp-json\/wp\/v2\/posts\/28258\/revisions"}],"predecessor-version":[{"id":42203,"href":"https:\/\/marketing.delta-engineering.be\/delta\/wp-json\/wp\/v2\/posts\/28258\/revisions\/42203"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/marketing.delta-engineering.be\/delta\/wp-json\/wp\/v2\/media\/42346"}],"wp:attachment":[{"href":"https:\/\/marketing.delta-engineering.be\/delta\/wp-json\/wp\/v2\/media?parent=28258"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/marketing.delta-engineering.be\/delta\/wp-json\/wp\/v2\/categories?post=28258"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/marketing.delta-engineering.be\/delta\/wp-json\/wp\/v2\/tags?post=28258"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}